LOCTITE ABLESTIK ECF 564A

Harmonization Code : 3920.99.28.90 | Other plates, sheets, film, foil and strip, of plastics, non-cellular and not reinforced, laminated, supported or similarly combined with other materials ; Of other plastics ; Other; Other

LOCTITE ABLESTIK ECF 564A

Main features

  • Electrically conductive
  • Excellent thermal conductivity
  • Passes Mil 5011 and NASA outgassing

Product Description

LOCTITE ABLESTIK ECF 564A adhesive film is designed for use in hybrid packages where outgassing and ionic contamination must be kept to a minimum. This electrically conductive adhesive film has excellent thermal conductivity and comes with a glass fabric carrier.

LOCTITE ABLESTIK ECF 564A assembly adhesive film has very low squeeze out during bonding and meets the NASA outgassing requirements and those of MIL-STD883C, Method 5011

 

Cure Schedule

  • 2 hours @ 150°C
Product Family

ABLESTIK ECF 564A

1. Select Package Type

Loading pricing…

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Glass Transition Temperature (Tg) Glass Transition Temperature (Tg)
150 °C
Thermal Conductivity Thermal Conductivity
2.2 W/m.K
Weight Loss @ 300°C Weight Loss @ 300°C
0.26 %