DCT-PO165 | Polyolefin Die Cutting Tape

Harmonization Code : 3920.10.89.90 | Other plates, sheets, film, foil and strip, of plastics, non-cellular and not reinforced, laminated, supported or similarly combined with other materials; Of polymers of ethylene; Of a thickness exceeding 0,125 mm; Other; Other; Other

DCT-PO165 | Polyolefin Die Cutting Tape

Main features

  • 165 µm film thickness
  • UV removable acrylic adhesive
  • Gentle adhesion for packaging substrates and glass

Product Description

LINQTAPE™ DCT-PO165 is a frosted polyolefin (PO) tape used in the dicing process. It provides an excellent balance of electrical, mechanical, thermal, and chemical properties. Compared to a PET dicing tape, PO dicing tapes have the same strong adhesion but are more easily removed from the substrate. This makes it ideal for applications such as packaging substrates, or delicate substrates where gentler adhesion is required for easier removal. 

LINQTAPE™ DCT-PO165 can be peeled by using UV. To ensure a clean substrate after removing the tape, DCT-PO165 utilizes a technology through which after applying UV light, the adhesive (18,600 N/25mm) becomes less tacky (180 N/25mm), which facilitates the removal of the tape. This quality makes the tape ideal for glass, sensitive substrates, and applications for which the final product must be clean of any residue. DCT-PO165 is a 150µm PO film, with a one-sided 15µm acrylic adhesive layer, and backed with a PET liner. This product can be customized according to the customer's needs. 

 

Key Features

  • Strong adhesion to prevent substrate damage
  • Can be used with uneven surfaces
  • Antistatic
  • High transparency
  • High flexibility
  • High chemical resistance 
  • No residue after removal

Application Ideas

  • Masking
  • Temporary bonding
  • Assembly of delicate components
  • Packaging substrates
  • Glass (e.g. optical applications)
Product Family

LINQ DCT-PO165

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Adhesive Layer Adhesive Layer
Acrylic
Adhesive Thickness Adhesive Thickness
15 µm
Appearance Appearance
Frosted
Release Liner Release Liner
Yes
Total Thickness Total Thickness
165 μm
Mechanical Properties
Adhesion Strength Adhesion Strength
66905 Oz/in
Elongation Elongation
941 lengthwise, 838 crosswise %
Tensile Strength (Thin Film) Tensile Strength (Thin Film)
34 lengthwise, 31 crosswise N/cm