LOCTITE AA 3936

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

LOCTITE 3936

Main features

  • Medium-Viscosity Gap Control
  • Sub-Five-Second Light Fixturing
  • Flexible Cannula Bonding

Product Description

LOCTITE AA 3936 is a one-component, medium-viscosity UV/visible-light acrylic adhesive for cannula bonding and precision medical-device assembly. The transparent-to-slightly-hazy liquid requires no mixing, fluoresces under UV light, and reaches fixture strength in under 5 seconds under the specified 365 nm light conditions. Its 8,000 to 14,000 mPa s viscosity is suited to dispensing adhesive on the cannula before hub assembly, larger cannula-to-hub gaps, and geometries where the cannula ends in the core pin bore. After cure, the material has 300% elongation and Shore D 55. Applications include hubs, syringes, and lancets using stainless steel cannulae.

Key features

  • Medium-Viscosity Placement: The 8,000 to 14,000 mPa s range supports pre-applied cannula adhesive and larger hub gaps.
  • Sub-Five-Second Fixture: Fixture strength develops in under 5 seconds at the listed 365 nm light conditions.
  • Flexible Cured Material: The cured adhesive provides 300% elongation with Shore D 55 hardness.

Applications / Suitable for

  • Bonding stainless steel cannulae into hubs
  • Larger-gap cannula-to-hub joints
  • Syringe and lancet needle assembly

Technical Specifications

General Properties
Specific Gravity Specific Gravity
1.1
Thermal Properties
Glass Transition Temperature (Tg) Glass Transition Temperature (Tg)
66 °C
Physical Properties
Tack-Free Time Tack-Free Time
>60 minutes
Viscosity Viscosity
8,000 to 14,000 mPa.s
Chemical Properties
Water Absorption Water Absorption
4.1 %
Mechanical Properties
Elongation Elongation
300 %

Additional Information

Technical properties

As-supplied / before-processing properties

Typical values for the uncured or as-supplied product unless otherwise noted.

PropertyValueUnitMethod / condition
AppearanceTransparent to slightly hazy-Uncured
UV fluorescencePositive-Uncured material under UV light
Specific gravity1.1-25 deg C
Viscosity8,000 to 14,000mPa sBrookfield RVT, spindle 5, 20 rpm, 25 deg C
Technical properties

After-processing / final-state properties

Typical values for the cured product under the listed methods and conditions.

PropertyValueUnitMethod / condition
Glass transition temperature66deg CASTM E 228; cured 30 seconds per side at 100 mW/cm^2 and 365 nm
Shore hardness55Durometer DISO 868; same cure
Elongation at break300%ISO 527-3; same cure
Tensile strength19N/mm^2ISO 527-3; same cure
Tensile modulus169N/mm^2ISO 527-3; same cure
Block shear strength19.0N/mm^2ISO 13445; polycarbonate to polycarbonate; cured 30 seconds at 100 mW/cm^2 and 365 nm